Alloy 233
Grade: Haynes 233/Alloy 233/Nickel Alloy 233
Sheet/Plate: 0.3mm-150mm
Strip/Foil: 0.02mm-16mm
Pipe: 6mm*0.5mm-1200mm*100mm
Bar: Ф6mm – Ф600mm
Wire: Ф0.01mm – Ф6mm
Others: Forged Rings, Flanges, Elbows, Tees, Reducers etc.
Standard: ASTM/ASME/AMS
- Fast Shipping / Ready Stock
- ISO 9001 Factory
- Custom Cutting
- 100% MTC & SGS Inspection
HAYNES 233 alloy is a new Ni-Co-Cr-Mo-Al alloy that offers excellent oxidation resistance at temperatures up to 2100°F (1149°C) or higher coupled with superior creep strength – a combination of properties never before achieved in a readily fabricable alloy. The alloy obtains its exceptional oxidation resistance through the formation of a protective alumina layer, while the high creep strength is a result of solid-solution and carbide strengthening. Additionally, for use in intermediate temperature applications the alloy can be age-hardened by heat treatment to produce even greater strength. Finally, the alloy can be readily fabricated using conventional methods since it exhibits good hot workability, cold formability, and weldability.
Chemical Composition
| Nickel | 48 (Balance) |
| Chromium | 19 |
| Cobalt | 19 |
| Molybdenum | 7.5 |
| Titanium | 0.5 |
| Aluminum | 3.3 |
| Iron | 1.5 max. |
| Manganese | 0.4 max. |
| Silicon | 0.20 max. |
| Carbon | 0.1 |
| Boron | 0.004 |
| Tantalum | 0.5 |
| Tungsten | 0.3 max. |
| Yttrium | 0.025 max. |
Tensile Properties (Age-Hardened)
| Temperature | 0.2% Yield Strength | Ultimate Tensile Strength | Elongation | |||
| °F | °C | ksi | MPa | ksi | MPa | % |
| RT | RT | 112.9 | 778 | 172.2 | 1187 | 27.3 |
| 1000 | 538 | 102.2 | 704 | 147 | 1014 | 25.8 |
| 1200 | 649 | 95.5 | 658 | 156.6 | 1079 | 25.5 |
| 1400 | 760 | 97.4 | 671 | 116.5 | 804 | 27.4 |
| 1500 | 816 | 82 | 565 | 92.3 | 637 | 21.6 |
Applications
▪ Hot gas components in aerospace and industrial gas turbines
▪ Industrial heating fixtures and sensors
▪ Various structural components in the emerging technology market.


HAYNES 233 alloy is a new Ni-Co-Cr-Mo-Al alloy that offers excellent oxidation resistance at temperatures up to 2100°F (1149°C) or higher coupled with superior creep strength – a combination of properties never before achieved in a readily fabricable alloy. The alloy obtains its exceptional oxidation resistance through the formation of a protective alumina layer, while the high creep strength is a result of solid-solution and carbide strengthening. Additionally, for use in intermediate temperature applications the alloy can be age-hardened by heat treatment to produce even greater strength. Finally, the alloy can be readily fabricated using conventional methods since it exhibits good hot workability, cold formability, and weldability.
Chemical Composition
| Nickel | 48 (Balance) |
| Chromium | 19 |
| Cobalt | 19 |
| Molybdenum | 7.5 |
| Titanium | 0.5 |
| Aluminum | 3.3 |
| Iron | 1.5 max. |
| Manganese | 0.4 max. |
| Silicon | 0.20 max. |
| Carbon | 0.1 |
| Boron | 0.004 |
| Tantalum | 0.5 |
| Tungsten | 0.3 max. |
| Yttrium | 0.025 max. |
Tensile Properties (Age-Hardened)
| Temperature | 0.2% Yield Strength | Ultimate Tensile Strength | Elongation | |||
| °F | °C | ksi | MPa | ksi | MPa | % |
| RT | RT | 112.9 | 778 | 172.2 | 1187 | 27.3 |
| 1000 | 538 | 102.2 | 704 | 147 | 1014 | 25.8 |
| 1200 | 649 | 95.5 | 658 | 156.6 | 1079 | 25.5 |
| 1400 | 760 | 97.4 | 671 | 116.5 | 804 | 27.4 |
| 1500 | 816 | 82 | 565 | 92.3 | 637 | 21.6 |
Applications
▪ Hot gas components in aerospace and industrial gas turbines
▪ Industrial heating fixtures and sensors
▪ Various structural components in the emerging technology market.
Related products
-
Incoloy
Alloy 840 / UNS S33400
-
Incoloy
Alloy 330/Incoloy 330
-
Nickel Alloy
Nickel 205/UNS N02205
-
Nickel Alloy
Nickel 200/UNS N02200
-
Nickel Alloy
Alloy 36/UNS K93600
-
Hastelloy
Alloy C22/UNS N06022