2507 Stainless Steel Flange
Grade: 2507/S32750 /S32760
Flange types:
Weld Neck (WN); Slip-On (SO); Blind (BL); Socket Weld (SW); Threaded (TH); Lap Joint (LJ); Orifice Flange where specified
- Fast Shipping / Ready Stock
- ISO 9001 Factory
- Custom Cutting
- 100% MTC & SGS Inspection
2507 is a super duplex stainless steel with high chromium, molybdenum and nitrogen contents. Its duplex microstructure provides very high strength together with excellent resistance to pitting, crevice corrosion and chloride stress corrosion cracking. It is intended for demanding corrosive services such as seawater, offshore oil and gas, chemical processing and desalination where conventional austenitic grades may not provide sufficient resistance.
Chemical Composition
| Element | Specified / Typical Range (wt. %) |
| C | ≤0.030 |
| Mn | ≤1.20 |
| Si | ≤0.80 |
| P | ≤0.035 |
| S | ≤0.020 |
| Cr | 24.0–26.0 |
| Ni | 6.0–8.0 |
| Mo | 3.0–5.0 |
| N | 0.24–0.32 |
| Cu | 0.50 max. |
| Fe | Balance |
Note: Values are presented as representative ASTM A182 grade requirements. The applicable standard edition and material certificate govern the final chemical limits.
Mechanical Properties
| Property | Minimum / Requirement |
| Tensile Strength, min. | 795 MPa |
| Yield Strength, 0.2%, min. | 550 MPa |
| Elongation, min. | 15% |
| Hardness | As specified by applicable standard / product condition |
- Offshore platforms and subsea systems
- Seawater and desalination plants
- Oil and gas processing
- Chemical and petrochemical equipment
- High-chloride and highly corrosive piping systems


2507 is a super duplex stainless steel with high chromium, molybdenum and nitrogen contents. Its duplex microstructure provides very high strength together with excellent resistance to pitting, crevice corrosion and chloride stress corrosion cracking. It is intended for demanding corrosive services such as seawater, offshore oil and gas, chemical processing and desalination where conventional austenitic grades may not provide sufficient resistance.
Chemical Composition
| Element | Specified / Typical Range (wt. %) |
| C | ≤0.030 |
| Mn | ≤1.20 |
| Si | ≤0.80 |
| P | ≤0.035 |
| S | ≤0.020 |
| Cr | 24.0–26.0 |
| Ni | 6.0–8.0 |
| Mo | 3.0–5.0 |
| N | 0.24–0.32 |
| Cu | 0.50 max. |
| Fe | Balance |
Note: Values are presented as representative ASTM A182 grade requirements. The applicable standard edition and material certificate govern the final chemical limits.
Mechanical Properties
| Property | Minimum / Requirement |
| Tensile Strength, min. | 795 MPa |
| Yield Strength, 0.2%, min. | 550 MPa |
| Elongation, min. | 15% |
| Hardness | As specified by applicable standard / product condition |
- Offshore platforms and subsea systems
- Seawater and desalination plants
- Oil and gas processing
- Chemical and petrochemical equipment
- High-chloride and highly corrosive piping systems
Related products
-
Duplex Stainless Steel
329 Duplex Stainless Steel Plate
-
300 Series Stainless Steel
316Ti/1.4571 Stainless Steel Plate
-
300 Series Stainless Steel
316N/316LN Stainless Steel Plate
-
300 Series Stainless Steel
309S/309H Stainless Steel Plate
-
300 Series Stainless Steel
321/321H Stainless Steel Plate
-
Stainless Steel
Stainless Steel Clad Plate