TP310H Stainless Steel Pipe

Grade: 310H/TP310H/UNS S31009/W.Nr.1.4845/SUS310HTP

Size:

Seamless: 6mm*1mm-720mm*50mm

Welded: 12mm*0.5mm-2000mm*100mm

Coiled: 4mm*0.3mm-32mm*3mm

Standard: ASTM A312, ASTM A213, ASME SA312, ASME SA213 etc.

Surface: No.1(Pickling), Bright(Polished)

TP310H is a high-carbon, high-chromium-nickel austenitic stainless steel designed for severe high-temperature environments. Containing 24%–26% chromium and 19%–22% nickel alongside 0.04%–0.10% carbon, it provides exceptional oxidation resistance up to 1100°C in continuous service and outstanding creep-rupture strength. Its fully austenitic microstructure resists sigma-phase embrittlement and thermal fatigue, making it ideal for extreme heat recovery, furnace components, and aggressive thermal processing.

Chemical Composition (wt%, ASTM A213 / A312)

C Mn P S Si Cr Ni Mo Other
0.04 – 0.10 ≤ 2.00 ≤ 0.045 ≤ 0.030 ≤ 1.00 24.0 – 26.0 19.0 – 22.0 — —

Mechanical & Thermal Properties (Solution Annealed Condition)

Property / Parameter Specification Requirement
Tensile Strength (min) ≥ 515 MPa (75 ksi)
Yield Strength, 0.2% Offset (min) ≥ 205 MPa (30 ksi)
Elongation in 2 in. / 50 mm (min) ≥ 35%
Hardness (max) ≤ 90 HRB / 192 HBW
Max Continuous Service Temp. ~1100°C (2010°F)

Typical Applications

  • Radiant tubes, muffles, and retorts in industrial heat-treatment furnaces
  • Coal gasification internals, fluidized-bed combustors, and kiln linings
  • High-temperature petrochemical reformer tubes and flare tips
  • Thermal oxidizers, incinerators, and waste-heat recovery recuperators

TP310H is a high-carbon, high-chromium-nickel austenitic stainless steel designed for severe high-temperature environments. Containing 24%–26% chromium and 19%–22% nickel alongside 0.04%–0.10% carbon, it provides exceptional oxidation resistance up to 1100°C in continuous service and outstanding creep-rupture strength. Its fully austenitic microstructure resists sigma-phase embrittlement and thermal fatigue, making it ideal for extreme heat recovery, furnace components, and aggressive thermal processing.

Chemical Composition (wt%, ASTM A213 / A312)

C Mn P S Si Cr Ni Mo Other
0.04 – 0.10 ≤ 2.00 ≤ 0.045 ≤ 0.030 ≤ 1.00 24.0 – 26.0 19.0 – 22.0 — —

Mechanical & Thermal Properties (Solution Annealed Condition)

Property / Parameter Specification Requirement
Tensile Strength (min) ≥ 515 MPa (75 ksi)
Yield Strength, 0.2% Offset (min) ≥ 205 MPa (30 ksi)
Elongation in 2 in. / 50 mm (min) ≥ 35%
Hardness (max) ≤ 90 HRB / 192 HBW
Max Continuous Service Temp. ~1100°C (2010°F)

Typical Applications

  • Radiant tubes, muffles, and retorts in industrial heat-treatment furnaces
  • Coal gasification internals, fluidized-bed combustors, and kiln linings
  • High-temperature petrochemical reformer tubes and flare tips
  • Thermal oxidizers, incinerators, and waste-heat recovery recuperators