309HCb Stainless Steel Plate

Grade: 309HCb/UNS S30941

Thickness: 3.0mm-200mm

Width: 1.5m/2.0m/2.2m/2.4m or as client’s requirement.

Standard: ASTM A240/A240M, ASME SA240/240M

Finish: No.1, Polished

Type 309HCb is a high-carbon, niobium-stabilized version of 309Cb. The controlled higher carbon range is intended to support elevated-temperature strength, while niobium improves structural stability by tying up carbon and limiting chromium-carbide precipitation. With approximately 23% chromium and 12–16% nickel, it offers oxidation resistance and is used for components that must retain strength and stability during prolonged high-temperature exposure.

Chemical Composition (wt. %)

Element Minimum Maximum
Carbon (C) 0.04 0.10
Manganese (Mn) — 2.00 max
Silicon (Si) — 0.75 max
Phosphorus (P) — 0.045 max
Sulfur (S) — 0.030 max
Chromium (Cr) 22.00 24.00
Nickel (Ni) 12.00 16.00
Niobium (Nb/Cb) 10 × C min 1.10 max
Iron (Fe) Balance Balance

Mechanical Properties (Annealed Plate, Sheet and Strip)

Property Requirement
Tensile Strength 515 MPa min
0.2% Yield Strength 205 MPa min
Elongation (50 mm) 40% min
Hardness 217 HBW max / 95 HRBW max

Typical Applications

  • High-temperature furnace components and radiant tubes
  • Heat-treatment baskets, trays and fixtures
  • Industrial boiler and thermal-processing equipment parts
  • High-temperature welded assemblies and supports
  • Petrochemical and power-plant components subject to sustained heat

Type 309HCb is a high-carbon, niobium-stabilized version of 309Cb. The controlled higher carbon range is intended to support elevated-temperature strength, while niobium improves structural stability by tying up carbon and limiting chromium-carbide precipitation. With approximately 23% chromium and 12–16% nickel, it offers oxidation resistance and is used for components that must retain strength and stability during prolonged high-temperature exposure.

Chemical Composition (wt. %)

Element Minimum Maximum
Carbon (C) 0.04 0.10
Manganese (Mn) — 2.00 max
Silicon (Si) — 0.75 max
Phosphorus (P) — 0.045 max
Sulfur (S) — 0.030 max
Chromium (Cr) 22.00 24.00
Nickel (Ni) 12.00 16.00
Niobium (Nb/Cb) 10 × C min 1.10 max
Iron (Fe) Balance Balance

Mechanical Properties (Annealed Plate, Sheet and Strip)

Property Requirement
Tensile Strength 515 MPa min
0.2% Yield Strength 205 MPa min
Elongation (50 mm) 40% min
Hardness 217 HBW max / 95 HRBW max

Typical Applications

  • High-temperature furnace components and radiant tubes
  • Heat-treatment baskets, trays and fixtures
  • Industrial boiler and thermal-processing equipment parts
  • High-temperature welded assemblies and supports
  • Petrochemical and power-plant components subject to sustained heat