304L Stainless Steel Seamless Pipe

Grade: 304L

Size:

Seamless: 6mm*1mm-720mm*50mm

Coiled: 4mm*0.5mm-32mm*3mm

Standard: ASTM A312, ASTM A213 etc.

Surface: No.1(Pickling), Bright(Polished)

304L Stainless Steel Pipe is a low-carbon austenitic stainless steel pipe offering excellent corrosion resistance, good weldability, and superior formability. With its low carbon content, 304L is particularly suitable for welded applications where resistance to intergranular corrosion is important. It is widely used in chemical, food, pharmaceutical, water treatment, and industrial piping systems.

Chemical Composition

Element Composition (%)
Carbon (C) ≤ 0.035
Silicon (Si) ≤ 1.00
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Chromium (Cr) 18.0–20.0
Nickel (Ni) 8.0–13.0
Molybdenum (Mo) —
Iron (Fe) Balance

Chemical composition is based on ASTM A312 TP304L requirements; specific values may vary according to the applicable product standard.

Mechanical Properties

Property Requirement
Tensile Strength ≥ 485 MPa
Yield Strength (0.2%) ≥ 170 MPa
Elongation ≥ 35%
Rockwell Hardness ≤ 92 HRB
Brinell Hardness ≤ 201 HB
Mechanical properties are typical minimum requirements for ASTM A312 TP304L stainless steel pipe.
  • Chemical Processing Equipment
  • Food & Beverage Processing
  • Pharmaceutical Equipment
  • Water Treatment Systems
  • Industrial Piping Systems
  • Oil & Gas Equipment
  • Petrochemical Industries
  • Heat Exchangers
  • Dairy Processing Equipment
  • Architectural & Structural Applications
  • Kitchen & Catering Equipment
  • General Fluid Transportation

304L Stainless Steel Pipe is a low-carbon austenitic stainless steel pipe offering excellent corrosion resistance, good weldability, and superior formability. With its low carbon content, 304L is particularly suitable for welded applications where resistance to intergranular corrosion is important. It is widely used in chemical, food, pharmaceutical, water treatment, and industrial piping systems.

Chemical Composition

Element Composition (%)
Carbon (C) ≤ 0.035
Silicon (Si) ≤ 1.00
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Chromium (Cr) 18.0–20.0
Nickel (Ni) 8.0–13.0
Molybdenum (Mo) —
Iron (Fe) Balance

Chemical composition is based on ASTM A312 TP304L requirements; specific values may vary according to the applicable product standard.

Mechanical Properties

Property Requirement
Tensile Strength ≥ 485 MPa
Yield Strength (0.2%) ≥ 170 MPa
Elongation ≥ 35%
Rockwell Hardness ≤ 92 HRB
Brinell Hardness ≤ 201 HB
Mechanical properties are typical minimum requirements for ASTM A312 TP304L stainless steel pipe.
  • Chemical Processing Equipment
  • Food & Beverage Processing
  • Pharmaceutical Equipment
  • Water Treatment Systems
  • Industrial Piping Systems
  • Oil & Gas Equipment
  • Petrochemical Industries
  • Heat Exchangers
  • Dairy Processing Equipment
  • Architectural & Structural Applications
  • Kitchen & Catering Equipment
  • General Fluid Transportation

Send Iquiry

Scroll to Top

Request a Quote

Name
Interested Products

Get Free Sample

Name
Interested Products