TP316H Stainless Steel Pipe

Grade: 316H/TP316H/UNS S31609/W.Nr.1.4918/SUS316HTP

Size:

Seamless: 6mm*1mm-720mm*50mm

Welded: 12mm*0.5mm-2000mm*100mm

Coiled: 4mm*0.3mm-32mm*3mm

Standard: ASTM A312, ASTM A213, ASME SA312, ASME SA213 etc.

Surface: No.1(Pickling), Bright(Polished)

TP316H is the high-carbon variant of molybdenum-bearing Type 316 austenitic stainless steel, formulated for enhanced elevated-temperature mechanical performance. The addition of 2.0%–3.0% molybdenum improves resistance to pitting, crevice corrosion, and sulfuric/organic acids, while the 0.04%–0.10% carbon range boosts short-term tensile strength and long-term creep rupture properties. It is widely specified where combined high-temperature strength and superior corrosion resistance are essential.

Chemical Composition (wt%, ASTM A213 / A312)

C Mn P S Si Cr Ni Mo Other
0.04 – 0.10 ≤ 2.00 ≤ 0.045 ≤ 0.030 ≤ 1.00 16.0 – 18.0 10.0 – 14.0 2.00 – 3.00 —

Mechanical & Thermal Properties (Solution Annealed Condition)

Property / Parameter Specification Requirement
Tensile Strength (min) ≥ 515 MPa (75 ksi)
Yield Strength, 0.2% Offset (min) ≥ 205 MPa (30 ksi)
Elongation in 2 in. / 50 mm (min) ≥ 35%
Hardness (max) ≤ 90 HRB / 192 HBW
Max Continuous Service Temp. ~815°C (1500°F)

Typical Applications

  • High-pressure superheater and reheater tubing in aggressive flue-gas environments
  • Chemical and pharmaceutical reactor coils, condensers, and heat exchangers
  • Pulp and paper digester heaters and marine/offshore thermal piping
  • Refinery hydrocracking and desulfurization high-temperature transfer lines

TP316H is the high-carbon variant of molybdenum-bearing Type 316 austenitic stainless steel, formulated for enhanced elevated-temperature mechanical performance. The addition of 2.0%–3.0% molybdenum improves resistance to pitting, crevice corrosion, and sulfuric/organic acids, while the 0.04%–0.10% carbon range boosts short-term tensile strength and long-term creep rupture properties. It is widely specified where combined high-temperature strength and superior corrosion resistance are essential.

Chemical Composition (wt%, ASTM A213 / A312)

C Mn P S Si Cr Ni Mo Other
0.04 – 0.10 ≤ 2.00 ≤ 0.045 ≤ 0.030 ≤ 1.00 16.0 – 18.0 10.0 – 14.0 2.00 – 3.00 —

Mechanical & Thermal Properties (Solution Annealed Condition)

Property / Parameter Specification Requirement
Tensile Strength (min) ≥ 515 MPa (75 ksi)
Yield Strength, 0.2% Offset (min) ≥ 205 MPa (30 ksi)
Elongation in 2 in. / 50 mm (min) ≥ 35%
Hardness (max) ≤ 90 HRB / 192 HBW
Max Continuous Service Temp. ~815°C (1500°F)

Typical Applications

  • High-pressure superheater and reheater tubing in aggressive flue-gas environments
  • Chemical and pharmaceutical reactor coils, condensers, and heat exchangers
  • Pulp and paper digester heaters and marine/offshore thermal piping
  • Refinery hydrocracking and desulfurization high-temperature transfer lines