309Cb Stainless Steel Plate
Grade: 309Cb/UNS S30940
Thickness: 3.0mm-200mm
Width: 1.5m/2.0m/2.2m/2.4m or as client’s requirement.
Standard: ASTM A240/A240M, ASME SA240/240M
Finish: No.1, Polished
- Fast Shipping / Ready Stock
- ISO 9001 Factory
- Custom Cutting
- 100% MTC & SGS Inspection
Type 309Cb is a niobium-stabilized, austenitic heat-resistant stainless steel with a chromium-nickel base. Its high chromium and nickel contents provide good resistance to oxidation and scaling at elevated temperatures, while niobium helps stabilize carbon and reduce the risk of chromium-carbide precipitation during service or welding. It is commonly selected for fabricated components exposed to high-temperature atmospheres and thermal cycling.
Chemical Composition (wt. %)
| Element | Minimum | Maximum |
| Carbon (C) | — | 0.08 max |
| Manganese (Mn) | — | 2.00 max |
| Silicon (Si) | — | 0.75 max |
| Phosphorus (P) | — | 0.045 max |
| Sulfur (S) | — | 0.030 max |
| Chromium (Cr) | 22.00 | 24.00 |
| Nickel (Ni) | 12.00 | 16.00 |
| Niobium (Nb/Cb) | 10 × C min | 1.10 max |
| Iron (Fe) | Balance | Balance |
Mechanical Properties (Annealed Plate, Sheet and Strip)
| Property | Requirement |
| Tensile Strength | 515 MPa min |
| 0.2% Yield Strength | 205 MPa min |
| Elongation (50 mm) | 40% min |
| Hardness | 217 HBW max / 95 HRBW max |
Typical Applications
- Furnace parts, furnace fixtures and heat-treatment equipment
- High-temperature ducts, exhaust components and expansion joints
- Combustion chambers, burner parts and thermal-processing equipment
- Welded fabrications operating under elevated-temperature conditions
- Petrochemical and power-generation equipment exposed to heat and oxidation


Type 309Cb is a niobium-stabilized, austenitic heat-resistant stainless steel with a chromium-nickel base. Its high chromium and nickel contents provide good resistance to oxidation and scaling at elevated temperatures, while niobium helps stabilize carbon and reduce the risk of chromium-carbide precipitation during service or welding. It is commonly selected for fabricated components exposed to high-temperature atmospheres and thermal cycling.
Chemical Composition (wt. %)
| Element | Minimum | Maximum |
| Carbon (C) | — | 0.08 max |
| Manganese (Mn) | — | 2.00 max |
| Silicon (Si) | — | 0.75 max |
| Phosphorus (P) | — | 0.045 max |
| Sulfur (S) | — | 0.030 max |
| Chromium (Cr) | 22.00 | 24.00 |
| Nickel (Ni) | 12.00 | 16.00 |
| Niobium (Nb/Cb) | 10 × C min | 1.10 max |
| Iron (Fe) | Balance | Balance |
Mechanical Properties (Annealed Plate, Sheet and Strip)
| Property | Requirement |
| Tensile Strength | 515 MPa min |
| 0.2% Yield Strength | 205 MPa min |
| Elongation (50 mm) | 40% min |
| Hardness | 217 HBW max / 95 HRBW max |
Typical Applications
- Furnace parts, furnace fixtures and heat-treatment equipment
- High-temperature ducts, exhaust components and expansion joints
- Combustion chambers, burner parts and thermal-processing equipment
- Welded fabrications operating under elevated-temperature conditions
- Petrochemical and power-generation equipment exposed to heat and oxidation
Related products
-
17-4 PH
630/17-4PH Stainless Steel Plate
-
300 Series Stainless Steel
316Ti/1.4571 Stainless Steel Plate
-
300 Series Stainless Steel
309S/309H Stainless Steel Plate
-
Stainless Steel
Stainless Steel Tube Sheet
-
Stainless Steel
Stainless Steel Embossed Sheet
-
Stainless Steel
Stainless Steel Thread Plate