TP321H Stainless Steel Pipe

Grade: 321H/TP321H/UNS S32109/W.Nr.1.4878/SUS321H

Size:

Seamless: 6mm*1mm-720mm*50mm

Welded: 12mm*0.5mm-2000mm*100mm

Coiled: 4mm*0.3mm-32mm*3mm

Standard: ASTM A312, ASTM A213, ASME SA312, ASME SA213 etc.

Surface: No.1(Pickling), Bright(Polished)

TP321H is a titanium-stabilized, high-carbon austenitic stainless steel tailored for high-temperature structural applications. Titanium additions (at least four times the carbon content, up to 0.70%) bind carbon as stable titanium carbides, preventing chromium carbide precipitation and intergranular corrosion within the 425°C–850°C sensitization range. Combined with 0.04%–0.10% carbon, TP321H offers excellent creep-rupture strength, fatigue resistance, and thermal stability in welded assemblies.

Chemical Composition (wt%, ASTM A213 / A312)

C Mn P S Si Cr Ni Mo Ti
0.04 – 0.10 ≤ 2.00 ≤ 0.045 ≤ 0.030 ≤ 1.00 17.0 – 19.0 9.0 – 12.0 — 4×C min – 0.70 max

Mechanical & Thermal Properties (Solution Annealed Condition)

Property / Parameter Specification Requirement
Tensile Strength (min) ≥ 515 MPa (75 ksi)
Yield Strength, 0.2% Offset (min) ≥ 205 MPa (30 ksi)
Elongation in 2 in. / 50 mm (min) ≥ 35%
Hardness (max) ≤ 90 HRB / 192 HBW
Max Continuous Service Temp. ~870°C (1600°F)

Typical Applications

  • Boiler superheater tubes and high-temperature steam headers subjected to thermal cycling
  • Aerospace exhaust manifolds, jet engine tailpipes, and expansion bellows
  • Refinery catalytic cracker internals, furnace tubes, and flare stacks
  • Welded high-temperature chemical equipment where post-weld annealing is impractical

TP321H is a titanium-stabilized, high-carbon austenitic stainless steel tailored for high-temperature structural applications. Titanium additions (at least four times the carbon content, up to 0.70%) bind carbon as stable titanium carbides, preventing chromium carbide precipitation and intergranular corrosion within the 425°C–850°C sensitization range. Combined with 0.04%–0.10% carbon, TP321H offers excellent creep-rupture strength, fatigue resistance, and thermal stability in welded assemblies.

Chemical Composition (wt%, ASTM A213 / A312)

C Mn P S Si Cr Ni Mo Ti
0.04 – 0.10 ≤ 2.00 ≤ 0.045 ≤ 0.030 ≤ 1.00 17.0 – 19.0 9.0 – 12.0 — 4×C min – 0.70 max

Mechanical & Thermal Properties (Solution Annealed Condition)

Property / Parameter Specification Requirement
Tensile Strength (min) ≥ 515 MPa (75 ksi)
Yield Strength, 0.2% Offset (min) ≥ 205 MPa (30 ksi)
Elongation in 2 in. / 50 mm (min) ≥ 35%
Hardness (max) ≤ 90 HRB / 192 HBW
Max Continuous Service Temp. ~870°C (1600°F)

Typical Applications

  • Boiler superheater tubes and high-temperature steam headers subjected to thermal cycling
  • Aerospace exhaust manifolds, jet engine tailpipes, and expansion bellows
  • Refinery catalytic cracker internals, furnace tubes, and flare stacks
  • Welded high-temperature chemical equipment where post-weld annealing is impractical
Translate »
Scroll to Top

Request a Quote

Name
Interested Products

Get Free Sample

Name
Interested Products