Product Name | Monel K-500 Alloy Sheet |
Brand | Tianjin Detai Co.,Ltd |
Payment Acceptable | T/T,L/C |
Port | Tianjin, Shanghai, Ningbo |
Package | Wooden package , less than 2 tons per cases |
Delivery time | within 15 working days |
Detect Metals is the leading Stainless Steel, Aluminum and other metal alloy manufacturer
Top Stainless Steel Plate Sheet Tube Pipe Coil supplier and exporter in China
Buy wholesale Monel K-500 Alloy Sheet from detect-metals.com at cheap factory price.
Monel K-500 Alloy Sheet
ASTM/AMS N05500 Alloy Sheet
EN 2.4375 Nickel based Alloy Sheet
Standard:
Bars, Wires and Forgings: ASTM B865, SAE AMS 4676, ISO 9725
Pipes: BS 3074NA18, DIN 17751
Sheets, Strip: BS3072NA18, BS3073NA18, ISO 6208, DIN 17750
Others: DIN 17743, SAE AMS 4676
Characteristics
Monel K500 is a Ni-Cu alloy with age-hardening properties imparted by alloying additions of aluminium and titanium. Its basic composition is similar to that of Monel 400 but the alloying additions make it age hardenable under controlled conditions of temperature and time.
Characteristics of Monel K500
After age-hardening of characeristics of Monel K500
Density: 8.47
Corrosion resistance
In general, the corrosion resistance of Monel K500 Alloy is similar to that of Monel 400 Alloy. Excellent resistance is shown to a wide range of media from pure water to mineral acids, salts and alkalis. Monel K500 Alloy is virtually immune to chloride-ion stress-corrosion cracking. In the aged condition, the alloy may be susceptible to stress-corrosion cracking in moist, aerated hydrofluoric acid vapour at stresses near the yield strength. In high-velocity seawater and in marine atmospheres, good corrosion resistance is shown but, in slow-moving or stagnant seawater, pitting may occur. Monel K500 Alloy also shows good resistance in sour-gas environments.
Applications
Monel K500 Alloy finds wide application in the marine, chemical, petrochemical and shipbuilding industries.
Typical applications are:
Chemical composition
Ni | Fe | C | Mn | Si | Cu | Al | Ti | S | P | Zn | Pb | Sn | |
min(%) | 63.0 | 27.0 | 2.30 | 0.35 | |||||||||
max(%) | 2.0 | 0.18 | 1.5 | 0.50 | 33.0 | 3.15 | 0.85 | 0.010 |
Mechanical properties
Condition | Yield Strength(Mpa) | Tensile Strength(Mpa) | Elongation(%) | Hardness(HB) | |
ASTM Min Value | Soft Annealed Aged | 690 | 965 | 20 | 265 |
Typical Values at RT | Hot worked Aged | 902 | 1078 | 25 | 305 |
Typical Values at RT | Cold worked Aged | 902 | 1078 | 22 | 310 |
Typical Values at RT | Soft Annealed Aged | 686 | 1000 | 28 | 285 |
International Specification Comparison chart
Material | Round Bar | Plate | |
ASTM | UNS N05500 |
B164 | |
ASME | |||
JIS | NW5500 | H4553 | H4551 |
DIN | 2.4375 | 17752 |
Product: Sheet, Coil, Pipe, Bar, Wire and Forgings